Gịnị Bụ Ihe Na-akpata nke PCB ịgbado ọkụ ntụpọ On Aluminom mkpụrụ PCB | YMS

Iji hụ na mkpokọta àgwà nke aluminum mkpụrụ PCB , na elu àgwà solder ga-eji na mmepụta usoro ka mma ịgbado ọkụ arụmọrụ nke PCB na gbochie warpage na ntụpọ. Soro ọkachamara PC aluminium PCB emepụta nke Yongmingsheng ịghọta.

1. Oghere weldability nke sekit osisi nwere mmetụta na ịgbado ọkụ àgwà.

N'ihi ire ere dara ogbenye nke oghere okirikiri, a ga-enwe ntụpọ ịgbado ọkụ mebere, na-emetụta akụkụ nke ihe ndị mejupụtara na sekit ahụ, na-akpata ihe ndị ahụ na akwa dị n'ime nke usoro nrụrụ na-enweghị nsogbu, na-ebute ọrụ zuru oke nke ọdịda sekit. .

2. eldgbado ọkụ ntụpọ na-akpata site n'ịgba agha.

Ogwe okirikiri na akụrụngwa ga-agbatị na usoro ịgbado ọkụ, na nrụgide na nrụrụ ga-eduga na ịgbado ọkụ mebere, obere eserese na ntụpọ ndị ọzọ.Warping na-ebutekarị site na nguzo ọkụ dị n'etiti akụkụ elu na nke ala nke bọọdụ okirikiri. polypropylene, bọọdụ ahụ na-ebu agha n'ihi ibu nke ya.

3. Nhazi nke bọọdụ sekit na-emetụta àgwà ịgbado ọkụ.

Site na echiche echiche, okirikiri nke sekit buru oke ibu, ọ bụ ezie ịgbado ọkụ dị mfe ịchịkwa, mana ahịrị ederede dị ogologo, impedance na-abawanye, ọnụahịa na-abawanye; Ogo ahụ pere mpe, ọkụ ọkụ na-ebelata, ịgbado ọkụ adịghị mfe ịchịkwa, na ibe nnyonye anya nke dị n'akụkụ edoghi mfe ime.

Ya mere imewe nke PCB osisi ga-kachasị:

A. Na-ebelata njikọta n'etiti ihe dị elu dị elu ma na-ebelata nnyonye aka nke electromagnetic.

B. Maka akụkụ dị arọ, dozie ha na brackets wee mezie ha.

C. Ihe ndị na-ekpo ọkụ kwesịrị ịtụle dị ka nsị ọkụ, ihe ndị na-ekpo ọkụ kwesịrị ịhapụ ebe ọkụ.

D. A na-ahazi ihe ndị ahụ n'otu oge dịka o kwere mee, nke na-abụghị naanị ọmarịcha, kamakwa ọ dị mfe ịgbado ọkụ ma dabara adaba maka imepụta ihe dị mma. Ihe kachasị mma maka bọọdụ sekit bụ 4∶3 rectangle. na mberede ma zere iji nnukwu mpaghara ọla kọpa.

The n'elu bụ ihe ịgbado ọkụ ntụpọ na PCB nke aluminom mkpụrụ. Enwere m olile anya na ọ nwere ike inye aka gị. Anyị si na China si soplaya na-emepụta soplaya - Yongmingsheng Electronics, kpọtụrụ!